The Truth About Stress Release in High MRR Machining

In the field of precision machining, especially when dealing with high-strength aluminum alloy extrusions such as 6061-T6 or 7075, a common efficiency misconception is that as long as the machine tool has sufficient rigidity and the cutting tools are advanced enough, one can pursue an unlimited increase in the MMR (metal removal rate).

However, reality often strikes a heavy blow to this idea. Many processors have encountered such a predicament: the dimensions of the part are perfect when measured in-machine and all tolerances are in the green; but after being placed for 24 hours or transferred to the next process, the originally parallel slots become narrower, or the positional accuracy of the multi-hole positions shifts. This phenomenon is commonly referred to in the industry as “part breathing”, and its physical essence is the re-balance and release of residual stresses within the material.

1. Deformation of the material structure after loosening the clamping

Here is a typical case we encountered during the processing of aluminum alloy:

The key to understanding this issue lies in observing a typical “stress-sensitive” structure. Take the following figure as an example. This aluminum alloy precision connector block perfectly demonstrates the challenge of stress release:

Aluminium part

The asymmetry of its geometric structure is the core of the challenge:

Central deep groove: It completely cuts off the original transverse fiber structure of the material and the continuous stress path.

Through holes: They further weaken the rigidity of the local area, forming weak points prone to stress concentration.

Side clamping seams: This is the most critical part. The release of internal stress is most likely to cause unpredictable dimensional drift at this location.

2. How does the high MMR processing break the physical equilibrium?

When you use large-diameter cutting tools to perform intense slotting to enhance efficiency, what you are doing is far more than “removing metal” – you are rapidly releasing the stored energy within the material.

After extrusion, there are already significant tensile or compressive residual stresses inside the aluminum material. In large removal rate processing, the external constraint layer is instantly removed, causing the stress field of the remaining part of the part to undergo a drastic reorganization to achieve a new mechanical balance. For parts like those shown in the figure with deep slots, the most common physical feedback is that the two sides of the slot mouth “close inward”, causing the meticulously maintained micrometer-level tolerance to fail instantly.

3. Thermal factors—Secondary stress caused by a sudden temperature rise 

In the case of high MMR processing, approximately 95% of the mechanical energy is converted into heat energy. [1] Although aluminum alloys have good thermal conductivity, extremely high instantaneous temperature gradients still occur at the cutting tip contact area during high-speed machining, leading to uneven micro thermal expansion. Studies have shown that during high-speed milling of aluminum alloys, the local instantaneous temperature at the cutting tip can reach several hundred degrees Celsius, which is sufficient to cause significant thermal plastic deformation at the microscopic level and is an additional stress source that cannot be ignored apart from mechanical stress.[2]

If the cooling is insufficient, this “thermal shock” will introduce new thermal residual stresses into the surface layer of the part. For the precision mating components in the above example diagram, the coupling of thermal stress and mechanical stress will eventually cause the part to undergo overall distortion after cooling. This also explains why the dimensional stability of the part under different seasonal environmental temperatures under the same process will vary.

4. Three core practical strategies for managing internal stress

To ensure the geometric stability of such high-precision parts, it is necessary to abandon the simplistic “one-step” approach and shift to a more intelligent stress management strategy.

Strategy 1: Stepwise stress relief and aging treatment

After the rough machining (in the high MRR stage), a 0.3-0.5mm allowance must be reserved. Then, perform the aging treatment. Even for urgent orders, the fixture should be loosened once on the machine to allow the material to “spring back” to its natural state before conducting the final fine machining.

Strategy 2: Symmetrical processing path

When processing the long slots of the parts in the example, avoid sequential cutting in a single direction. It is recommended to adopt a symmetrical cutting logic that extends from the center to both ends, so that the stress can be evenly released on both sides and avoid accumulation on a single side.

Strategy 3: Optimizing Cutting Ratio Energy and Tool Selection

From a physics standpoint, reducing cutting forces means reducing the deformation energy introduced into the workpiece. Therefore, it is advisable to preferentially select special polishing aluminum tools with a high rake angle and extremely sharp cutting edges, to cut the material in the most “gentle” manner, and to suppress the generation of new stresses at the source.

The essence of precision machining is not merely the removal of materials, but rather a battle with the internal physical properties of the materials. The next time you plan to challenge a higher metal removal rate, pause for a moment and think: Has your process design provided sufficient “breathing room” for that invisible yet inevitable internal stress?

tristan.zhou

Rapid manufacturing engineer with over 15 years of hands-on experience in CNC machining, injection molding, sheet metal fabrication, vacuum casting, and industrial 3D printing.

Focused on sharing practical insights into prototyping, product development, and manufacturing solutions to help engineers and businesses bring products to market faster.

Scroll to Top