Delrin vs Nylon: Properties, Machinability, and Applications

Delrin and Nylon are widely used engineering plastics for gears, bushings, rollers, and other mechanical parts. While they share many applications, differences in their material properties and machining performance affect how parts perform in service. Understanding these differences helps engineers select the right material for their projects.

What Are Delrin and Nylon?

Delrin is a brand of acetal homopolymer, also known as POM-H (polyoxymethylene homopolymer). It offers high stiffness, low friction, excellent fatigue resistance, and good dimensional stability. These properties make Delrin a common material for precision gears, bushings, valve components, and moving mechanical parts.

Delrin belongs to the broader polyoxymethylene (POM) family, which also includes acetal copolymer (POM-C). POM-H generally offers higher stiffness and strength, while POM-C provides better resistance to certain chemicals and improved processing stability. Delrin is a specific brand of POM-H rather than a general name for all acetal plastics.

Nylon is a family of polyamide (PA) thermoplastics known for toughness, wear resistance, mechanical strength, and versatility. Unlike Delrin, Nylon includes several grades with different properties and manufacturing characteristics.

Material grade Key characteristics Common applications
Delrin (POM-H)High stiffness, low friction, excellent machinabilityPrecision gears, bushings, valve parts
POM-CGood chemical resistance and dimensional stabilityPump components, fittings, mechanical parts
PA6 (Nylon 6)Good toughness, strength, and wear resistanceRollers, gears, guides
PA66 (Nylon 66)High stiffness, strength, and thermal resistanceMechanical components, gears, brackets
PA6C (Cast Nylon 6)Good wear resistance and impact performance; available in large stock sizesIndustrial rollers, pulleys, wear pads
PA12 (Nylon 12)Lower moisture absorption than PA6 and PA66, good flexibilityFunctional prototypes, tubing, 3D printed parts
Glass-Filled NylonIncreased stiffness, strength, and creep resistanceStructural supports, automotive parts
Oil-Filled NylonImproved sliding and wear performanceBushings, bearings, industrial guides

Different Nylon grades are designed for different requirements. PA66 provides greater stiffness than many general-purpose PA12 grades, while cast Nylon 6 is widely used for large industrial components. PA12 is particularly useful where reduced moisture absorption and additive manufacturing compatibility are important.

The differences between POM-H, POM-C, and the various Nylon grades should be considered before selecting a material for production.

Delrin vs Nylon: Key Property Differences

Delrin and Nylon share several mechanical characteristics, but their performance changes under different operating conditions. Moisture exposure, mechanical loading, temperature, and friction are especially important for precision components.

Mechanical Strength, Stiffness, and Impact Resistance

Delrin provides high stiffness and good fatigue resistance, making it well suited for components that require consistent geometry under repeated mechanical movement. Nylon is known for toughness and impact resistance, particularly in applications involving vibration, shock loading, and industrial wear.

However, strength is not the same as toughness. A material with higher tensile strength does not necessarily perform better under impact loading. Nylon also changes its mechanical behavior as it absorbs moisture, so dry and conditioned material properties should not be treated as equivalent.

The following values illustrate differences between specific commercial stock materials.

Property Delrin PA6 PA66 PA12
Density (g/cm³) 1.421.141.141.02
Tensile strength (MPa) 697983 (yield)53
Tensile modulus (MPa) 3,1033,3002,4131,800
Elongation at break (%) 7513050200
Approx. melting temperature (°C) 175221255180

The table also shows why material grade matters. PA12, for example, has lower stiffness than the listed PA6 grade but much greater elongation at break. Glass-filled Nylon increases stiffness substantially, although it generally reduces ductility compared with the corresponding unfilled material.

For highly loaded components, tensile properties should be reviewed together with impact resistance, fatigue performance, and long-term creep.

Moisture Absorption and Dimensional Stability

Moisture absorption is one of the most important differences between Delrin and conventional Nylon grades.

Nylon absorbs moisture from the surrounding environment. As its moisture content increases, the material expands and its stiffness changes. These changes are particularly important for precision components with tight-fitting features.

Consider a Nylon bushing machined to fit inside a metal housing. The bushing can meet its specified dimensions immediately after machining, but moisture absorption during storage or operation can increase its diameter and reduce the available assembly clearance.

Delrin absorbs considerably less moisture than common PA6 and PA66 materials, giving it better dimensional stability under changing humidity.

Published material data illustrate this difference:

Material 24-hour water absorption Test reference
Typical Delrin stock0.25%ASTM D570
TECAMID 6 natural (PA6)0.30%DIN EN ISO 62, 23°C
TECAMID 66 natural (PA66)0.45%ASTM D570, 23°C
TECAMID 12 natural (PA12)0.04%DIN EN ISO 62, 23°C

How much can moisture affect a precision part?

Take a Nylon bushing with a nominal outside diameter of 20 mm. If its diameter increases by an assumed 0.3% after moisture conditioning, the dimensional change is:

20 mm × 0.003 = 0.06 mm

The bushing’s diameter becomes approximately 20.06 mm. If the assembly originally had only 0.03 mm of diametral clearance, this increase would eliminate the clearance and create interference.

The 0.3% dimensional change is an illustrative assumption, not a universal expansion rate for Nylon. Actual expansion depends on the material grade, moisture content, part geometry, and environmental conditions.

For precision machined Nylon components, the material’s moisture condition should be considered when defining tolerances and inspection requirements.

Friction, Wear Resistance, and Heat Performance

Delrin has a naturally low coefficient of friction and good wear resistance. It is widely used in precision gears, sliding mechanisms, and moving parts where consistent movement and dimensional accuracy are important.

Nylon also provides excellent wear performance in industrial applications. Cast Nylon 6 is widely used for rollers, pulleys, guides, and wear pads, while oil-filled grades are designed for sliding components where external lubrication is limited.

Actual wear performance depends on contact pressure, sliding speed, lubrication, and the mating surface. These operating conditions are more useful for material selection than a general claim that one material is more wear-resistant.

Temperature is another important consideration. Standard Delrin performs well in many moderate-temperature mechanical applications. PA66 has a higher melting temperature, while reinforced and heat-stabilized Nylon grades provide additional options for elevated-temperature service.

Melting temperature, heat deflection temperature, and continuous service temperature describe different properties. A higher melting point does not automatically mean better performance under sustained mechanical loading.

Chemical exposure also affects material selection. Delrin resists many common oils, fuels, and solvents, while Nylon offers good resistance to many industrial lubricants and oils. Strong acids and other aggressive chemicals require careful compatibility checks for both materials.

Delrin vs Nylon for CNC Machining and Manufacturing

Delrin is widely used for precision CNC machining because of its stiffness, clean chip formation, and dimensional stability. It is a reliable material for machined gears, bushings, spacers, and mechanical components with closely controlled features.

Nylon is also a common CNC machining material, particularly for rollers, wear pads, guides, and larger industrial components. However, its greater elasticity and moisture sensitivity create additional machining considerations.

Machinability, Surface Finish, and Tolerances

Delrin cuts cleanly with sharp tools and suitable machining parameters. Its relatively rigid structure helps maintain well-defined edges and smooth surfaces during milling and turning.

Nylon can produce long, stringy chips and develop burrs around holes, slots, and edges. Tool geometry, chip removal, and cutting conditions therefore play an important role in maintaining a consistent finish.

Machining factor Delrin Nylon
Chip formationClean, consistent chipsOften longer, stringy chips
Burr formationGenerally easier to controlMore attention to deburring
Dimensional stabilityLower moisture sensitivityMoisture conditioning affects dimensions
Thin-wall machiningGood stability with suitable clampingGreater elastic deflection under clamping
Surface finishSmooth machined surfaces readily achievableRequires appropriate tools and cutting parameters
Typical CNC applicationsPrecision gears, bushings, valve partsRollers, guides, wear pads, structural parts

Workholding is particularly important for thin-walled plastic components. For example, excessive clamping pressure can temporarily distort a Nylon sleeve during machining. Once the part is removed from the fixture, elastic recovery changes its final measured dimensions.

The solution is to control clamping pressure, use suitable cutting parameters, and allow for material stabilization when the application requires it. These practices also benefit Delrin components, especially when large amounts of material are removed.

For B2B manufacturing projects, engineering drawings should clearly specify the required material grade. A drawing that simply states “Nylon” leaves substantial room for interpretation because PA6, PA66, PA12, and filled grades have different properties.

Similarly, “POM” does not identify whether the required material is POM-H or POM-C. The grade, reinforcement, and relevant material specification should be identified before production.

For close-tolerance Nylon parts, the drawing or purchase specification should also establish the expected conditioning and inspection environment.

Which Material Is More Cost-Effective?

Raw material price is only one part of the manufacturing cost.

Certain Nylon grades and stock sizes are less expensive than Delrin, but additional machining operations, deburring, stabilization, and dimensional inspection can affect the final quote.

Delrin’s predictable machining behavior makes it cost-effective for many precision components. Nylon remains an economical material for industrial rollers, guides, and structural parts, particularly when the selected grade and tolerance requirements match the application.

Stock size also matters. Cast Nylon is available in large rods, plates, and tubes, making it a practical option for substantial industrial components.

For purchasing decisions, the relevant figure is the total cost of a finished part that meets the drawing requirements, including material, machining, inspection, and production quantity.

CNC Machining, Injection Molding, and 3D Printing

Both Delrin and Nylon are used in CNC machining and injection molding. However, they offer different options for additive manufacturing.

Nylon is widely used in industrial 3D printing. PA11 and PA12 are established materials for selective laser sintering (SLS) and Multi Jet Fusion (MJF), supporting functional prototypes and complex geometries.

Delrin is not commonly used in standard 3D printing workflows. POM filament printing is technically possible, but warping, processing control, and thermal decomposition risks make it significantly less common than Nylon printing.

For projects involving functional 3D printed prototypes, Nylon provides a well-established material range. Delrin remains particularly useful when the project requires precisely machined components with stable mechanical dimensions.

Common Industrial Applications

Both materials are used across automotive equipment, industrial machinery, product development, and precision mechanical assemblies. Their suitability becomes clearer when evaluated by component type.

Gears: Delrin is commonly used for small precision gears because of its low friction, dimensional stability, and fatigue resistance. Nylon gears are widely used in machinery where impact resistance, vibration damping, and quieter operation are important.

Bushings and bearings: Delrin provides stable dimensions for close-fitting bushings and sliding components. Cast and lubricated Nylon grades are established choices for heavily loaded industrial bearings and wear applications.

Industrial rollers and pulleys: Cast Nylon 6 is a standard material for larger rollers, pulleys, sheaves, and wear pads. Its toughness, damping behavior, and availability in large stock sizes support these applications.

Mechanical structural components: PA66 and glass-filled Nylon are widely used for brackets, housings, and mechanical supports. Delrin is frequently selected for components requiring consistent dimensions and controlled mechanical movement.

Pump and valve components: Delrin is used for precision valve parts, fittings, and fluid-handling components where low moisture absorption is valuable. Chemical compatibility must still be confirmed for the specific fluid and operating temperature.

Component requirement Common material choice
Small precision gearDelrin
Industrial impact-resistant rollerCast Nylon
Close-tolerance bushing in humid conditionsDelrin
Heavy-duty wear padCast or modified Nylon
Structural bracket requiring high stiffnessPA66 or glass-filled Nylon
Precision sliding componentDelrin
Complex functional 3D printed partPA11 or PA12

These choices reflect common manufacturing practice. Final selection should be based on actual loads, operating conditions, the specific material grade, and the required component life.

How to Choose Between Delrin and Nylon

The selection process starts with the component’s operating requirements.

For precision parts exposed to changing humidity, Delrin provides a strong combination of dimensional stability, low friction, and machinability. It is particularly useful for close-fitting gears, bushings, and mechanical components.

For applications involving impact, vibration, large wear surfaces, or heavy industrial movement, Nylon offers a wide selection of suitable grades. PA6C is established in large wear components, PA66 is used for stronger structural applications, and PA12 provides additional advantages in moisture-sensitive and additive manufacturing projects.

Manufacturing requirements are equally important. CNC machining, injection molding, and 3D printing each place different demands on the material. The selected grade should match both the final operating conditions and the intended production process.

A reliable material choice considers performance, dimensional stability, production cost, and long-term service requirements together.

Frequently Asked Questions

Is Delrin stronger than Nylon?

Strength depends on the specific grade and testing conditions. Some dry Nylon grades have higher tensile strength than standard Delrin, while Delrin provides more consistent dimensional behavior under changing humidity. Stiffness, impact resistance, and long-term loading also influence the comparison.

Is Delrin or Nylon better for gears?

Delrin is widely used for precision gears requiring stable dimensions and low friction. Nylon is common in gears that benefit from toughness, impact resistance, and vibration damping. The final choice depends on tooth loading, lubrication, temperature, and operating conditions.

Which is easier to CNC machine, Delrin or Nylon?

Delrin generally machines more cleanly and predictably. Nylon is also suitable for CNC machining but requires greater attention to burr formation, workholding, moisture conditioning, and dimensional control.

Can Nylon replace Delrin in mechanical parts?

Nylon can replace Delrin in applications where its mechanical properties and dimensional behavior meet the design requirements. The specific grade, operating environment, assembly clearance, and wear conditions must be checked before substitution.

tristan.zhou

Rapid manufacturing engineer with over 15 years of hands-on experience in CNC machining, injection molding, sheet metal fabrication, vacuum casting, and industrial 3D printing.

Focused on sharing practical insights into prototyping, product development, and manufacturing solutions to help engineers and businesses bring products to market faster.